Author Topic: electroplating prep.  (Read 14482 times)
Ed
Guru
*****
Offline Offline

Model: FE
Posts: 3311



Ed74mnd
View Profile
« Reply #20 on: August 08, 2007, 08:46:10 AM »
0

Sorry i don't know a chemical that would strip chrome, I dare say it would be extremely toxic and difficult to handle.

got the zinced parts back today and everything is great, except I sent the tailgate struts (upper) to be plated and the process has killed the die cast switch in the latch, so I guess these are now useless...

anybody got some nice tailgate struts uppers?

otherwise gas struts?

Cheers

Ed


Logged

in the shed
Rabbitoh
vic-club
Senior Member
****
Offline Offline

Model: FE
Posts: 522


FE - 'King of Cars'


View Profile
« Reply #21 on: September 11, 2007, 01:20:23 PM »
0

add the molasses to around 8 liters of water to 1 litre of mollasses. Mix well and wait about two weeks depending on the temperature where you live. The mollasses starts to ferment and smell like dog turds ( true ).  A chemical reaction occurs bettween the rust and the fermented mollasses.It takes bettween 4 and 6 weeks depending on the severity of the rust .
Confirmation please, do you need to leave solution sitting for 2 weeks prior to dipping parts in, or can you plop 'em in at the start?
Logged

Fortius Quo Fidelius 1966; Saints' 2nd in 2025?
Bunnies' 22nd in 2025?
sgo
Senior Member
****
Offline Offline

Posts: 444



View Profile WWW
« Reply #22 on: September 11, 2007, 06:32:25 PM »
0

Mix it up, remove all paint and grease from parts, tie them to a wire and hang them in, submerged.
Check them every few days for progress and most bits will be done by 2 weeks.
Hose them down at any stage to see how the're going and at the end.
Logged

mitchy
Newbie
*
Offline Offline

Posts: 19


I love YaBB 1G - SP1!


View Profile
« Reply #23 on: October 02, 2007, 08:57:46 PM »
0

   hi ed go to your local supermarket buy i plastic container of costic soda  i large bucket  empty contents of costic into bucket fill bucket with cold water only  add your part leave for a few days hose paint off . place part into same size bucket of cleaning vinigar from local supermarket leave for few days hose of should now be ready for chrome or paint regards mitch ( brookvale )
Logged
Ed
Guru
*****
Offline Offline

Model: FE
Posts: 3311



Ed74mnd
View Profile
« Reply #24 on: October 03, 2007, 07:53:51 AM »
0

Hey Mitch,

Great to hear from you again,
I did exactly what you described and it worked a treat, I should post some pics of the end result after zinc plating.  The hardest paint to shift was the etch primer, the top coats literally fell off but I had to gently scrub the etch primer away.

Cheers

Ed

Logged

in the shed
Pages: 1 [2]   Go Up
  Add bookmark  |  Print  

Share this topic...
In a forum (BBCode) 
In a site/blog (HTML)

 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.21 | SMF © 2015, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.032 seconds with 20 queries.