News:

Are you a member of one of the FE-FC Holden Car Clubs of Australia ? If you are, get access to the Club-Member-only area of this discussion board. Send an IM to the board admin, including your real name and club to get access.

Main Menu

nickle plating in Melbourne

Started by John253a, December 24, 2011, 01:10:52 PM

Previous topic - Next topic

John253a

looking to nickle plate (not chrome) all my bars and trim,
rang around and there a few that still do it, but none that want to touch the die-cast stuff

my question is do any of you no any that's doing it, that you would recommend,

tried to get hold of geelong electroplating (as they seem to be well recommended) but due to christmas it think the may have close for the holidays

John253a

Still looking for a good nickel plater in Vic.
Any recommendation 

Glenn 'Stinky' Stankevicius

I thought Nickel Plating was the last step before Chrome in the Chrome Plating process  ???

John253a

Not sure how they do it
I just like the look over chrome,

Had some bars nickel plated in sunshine back in 02 sometime and wasn't happy with there quality, 

KFH

According to the chap that did my plating there is a coat of copper first and if that won't remove all scratches when polished there is another coat of copper or more until all scratches are gone after polishing.  This is followed by a coat of Nickel then a coat of Chrome.

Keith
I was born with nothing and still have most of it left